DOES SMAW PROCESS CAN USE FOR ALUMINUM BUS BAR WELDING
DOES SMAW PROCESS CAN USE FOR ALUMINUM BUS BAR WELDING
(OP)
hi,
we have Electrical bus bar welding with 40mm fillet size.whether SMAW can use for Aluminum Bus bar welding and SMAW process welding can weld with DC current.
we have Electrical bus bar welding with 40mm fillet size.whether SMAW can use for Aluminum Bus bar welding and SMAW process welding can weld with DC current.





RE: DOES SMAW PROCESS CAN USE FOR ALUMINUM BUS BAR WELDING
RE: DOES SMAW PROCESS CAN USE FOR ALUMINUM BUS BAR WELDING
The flux is highly corrosive, so it must be completely removed at the conclusion of welding. Chip, wire brush, and flush with warm water to ensure its complete removal.
I have some aluminum welds made nearly 50 years ago made with SMAW. Once ground smooth, no one will know what they looked like in their as-welded state. Ty are still intact and serving their original purpose.
Best regards - Al
RE: DOES SMAW PROCESS CAN USE FOR ALUMINUM BUS BAR WELDING
RE: DOES SMAW PROCESS CAN USE FOR ALUMINUM BUS BAR WELDING
RE: DOES SMAW PROCESS CAN USE FOR ALUMINUM BUS BAR WELDING
RE: DOES SMAW PROCESS CAN USE FOR ALUMINUM BUS BAR WELDING
Best regards - Al