NACE spec for Chemical Processing Plants (similar to MR0175 for refineries)
NACE spec for Chemical Processing Plants (similar to MR0175 for refineries)
(OP)
Is there a NACE spec that covers material requirements for Chemical Processing plants?
(something similar to NACE MR0175 for Refineries?)
Thank You.
(something similar to NACE MR0175 for Refineries?)
Thank You.





RE: NACE spec for Chemical Processing Plants (similar to MR0175 for refineries)
RE: NACE spec for Chemical Processing Plants (similar to MR0175 for refineries)
MR0103-2012 is titled "Materials Resistant to Sulfide Stress Cracking in Corrosive Petroleum Refining Environments"
Are you aware of a NACE standard similar (to MR0103) that applies to Chemical Processing environments?
Thank You.
RE: NACE spec for Chemical Processing Plants (similar to MR0175 for refineries)
Thanks.
Pradip Goswami,P.Eng.IWE
Welding & Metallurgical Specialist
Ontario, Canada.
ca.linkedin.com/pub/pradip-goswami/5/985/299