Material group 5 Cr - 1/2 mo High alloy material UHA
Material group 5 Cr - 1/2 mo High alloy material UHA
(OP)
Hello:
It seems for me that it does not include 5 Gr-1/2 mo ( P5B- Gr 1 ) group material into Table UHA-32. Does it mean that 5 Gr- 1/2 mo group material not consider as high alloy materail , so the requirement as per UHA does not apply for it. Please clarify .
Thanks
Abraham Hong
It seems for me that it does not include 5 Gr-1/2 mo ( P5B- Gr 1 ) group material into Table UHA-32. Does it mean that 5 Gr- 1/2 mo group material not consider as high alloy materail , so the requirement as per UHA does not apply for it. Please clarify .
Thanks
Abraham Hong





RE: Material group 5 Cr - 1/2 mo High alloy material UHA
RE: Material group 5 Cr - 1/2 mo High alloy material UHA
Regards,
Mike