INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Purging Of Nitrogen

Purging Of Nitrogen

Purging Of Nitrogen

(OP)
After Hot bent of SA335 P91, we carried out Normalizing at 1038 degree Celsius and found oxidation/Scale inside Pipe which was difficult to remove. Decided to purge with Argon and found the result is ok ( No Scale). Due to economy, we are now planning for Nitrogen purging instead of Argon.
Whether Nitrogen purging at that Temp will affect any Mechanical/Metallurgical Properties, if so What??[/b]

RE: Purging Of Nitrogen

You are talking about the Nitrogen purging during Welding ?

Regards
Aakash Jha

RE: Purging Of Nitrogen

A protective atmosphere of nitrogen gas during normalizing will not harm the Grade 91.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources