INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

What is the heat treatment H04 for phosphor bronze?

What is the heat treatment H04 for phosphor bronze?

What is the heat treatment H04 for phosphor bronze?

(OP)
Hello,

I want to melt some phosphor bronze alloy and they requested H04 grade.

It is my first contact with this designation. Is it a heat treatment? If yes would you please recommend a place to find it?

Or does it mean cold work?

Thanks,

HErc

RE: What is the heat treatment H04 for phosphor bronze?

You are correct, H04 is a cold work designation (full hard).

Se ASTM B601 for additional information. You will probably have to find out what the requirements are for the "full hard" designation of the specific phosphor bronze alloy you are being asked to provide.

rp

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources