I am looking for a reference that gives guidance for describing corrosion based on visual inspections. For example, I am trying to figure out when you would quantify corrosion as being light, moderate, very corroded, severe, etc.
Thanks
Thanks





RE: Quantifying Levels of Corrosion based on Visual Inspection
http://www.astm.org/COMMIT/SUBCOMMIT/D0125.htm
ASTM D610 Standard Practice for Evaluating Degree of Rusting on Painted Steel Surfaces seems most appropriate.