INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Anyone know where I can find some "Bayer 348-012002 Lustran" stock?

Anyone know where I can find some "Bayer 348-012002 Lustran" stock?

Anyone know where I can find some "Bayer 348-012002 Lustran" stock?

(OP)
Just as the title says... any hints?

RE: Anyone know where I can find some "Bayer 348-012002 Lustran" stock?

Matweb lists it here with a button for supplier links:
http://www.matweb.com/search/DataSheet.aspx?MatGUI...

Supplier listed is: Stern & Co. Inc. is a distributor of plastic resin and sheet. We specialize in polystyrene, polypropylene, polyethylene, ABS, SAN, and PET. We inventory prime and widespec resins nationwide. We sell hips, coex, pet, rpet, and pp sheet and rollstock. To locate a sales office close to you, please call us at 732-382-9666, or fax us at 732-382-0054. You can visit our web site at www.isternplastics.com.

Or call INEOS for a list of their distributors. Or, as ABS is a commodity, use MatWeb to find an alternate grade from Dow, BASF etc..

Chris DeArmitt

Expert consulting & training
www.phantomplastics.com

RE: Anyone know where I can find some "Bayer 348-012002 Lustran" stock?

(OP)
Thank you! Very helpful materials website...

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources