INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Standard for aluminum T6 7075

Standard for aluminum T6 7075

Standard for aluminum T6 7075

(OP)
Hello all,

Is there a ANSI/ASME/ISO or other standard for taking 7075 T0 and tempering to T6? Our facility is trying to bring the tempering process of our aluminum in-house and we are looking for a standard to get us started.

Thank you for your time

RE: Standard for aluminum T6 7075

You need to obtain a copy of AMS 2770. In rough numbers, if you are starting with condition O, you will be solution treating anywhere from 880-915F, depending on product form. Water quench, then age at 250F for 24 hours.

RE: Standard for aluminum T6 7075

(OP)
Thank you very much!

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources