INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

ABQ_PLY_FABRIC User Subroutine

ABQ_PLY_FABRIC User Subroutine

ABQ_PLY_FABRIC User Subroutine

(OP)
Hi Everyone,

I am running into some trouble trying to use Abaqus' built-in user subroutine ABQ_PLY_FABRIC to model ply failure in woven carbon fiber composite. I built the model in Abaqus CAE and modified the input code to change the material to ABQ_PLY_FABRIC according to the Abaqus document as follows:

*MATERIAL, NAME = ABQ_PLY_FABRIC_1
*DENSITY
ρ
*USER MATERIAL, CONSTANTS = 40
** Line 1:
E1+, E2+, ν12+, E1-, E2-, ν12-
** Line 2:
X1+, X1-, X2+, X2-, S
** Line 3:
Gf1+, Gf1-, Gf2+, Gf2-, α12, dmax12
** Line 4:
σy0, C, p
** Line 5
lDelFlag, dmax, εplmax, εmax, εmin
*DEPVAR, DELETE = 16
16

The problem is I would always get this error message:
***ERROR: THE SOLUTION-DEPENDENT STATE VARIABLE INDEX MUST BE GREATER THAN 0 AND LESS THAN OR EQUAL TO 16
***NOTE: DUE TO AN INPUT ERROR THE ANALYSIS PRE-PROCESSOR HAS BEEN UNABLE TO INTERPRET SOME DATA. SUBSEQUENT ERRORS MAY BE CAUSED BY THIS OMISSION

I am attaching the Abaqus document that explains how to use this subroutine and my own input file of a single element with this material definition. I am not familiar with coding in Abaqus and would appreciate any advice on the matter. Thank you in advance.

ZhiMing

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources