INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

does anyone know DIN standard for Stellite 6R?

does anyone know DIN standard for Stellite 6R?

does anyone know DIN standard for Stellite 6R?

(OP)
Can anyone help me with the DIN Standard number for Stellite 6R?  Cheers, Torsten.

RE: does anyone know DIN standard for Stellite 6R?

The Deloro Stellite website listed the following specifications for Stellite 6:

SAE AMS 5387
SAE AMS 5373
AWS 5.13 RCoCr-A
UNS 30006

I am not aware of any DIN norms that cover cobalt-based alloys.  I will perform a search and let you know if I find anything.  In the meantime, you may try contacting someone at Deloro Stellite with this question.  The website is http://www.stellite.com.

RE: does anyone know DIN standard for Stellite 6R?

(OP)
Thank you for your answer and your help...I am really struggling here...we use Stellite coated wedges within our equipment and I am having a German customer, who is insisting on being told the DIN standard number for this and I just can't get it anywhere...Cheers (from Liverpool), Torsten.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources