AL-6XN (UNS-N08367), can it be used as a coil material inside a boiler(Complying with Sec I) ?
AL-6XN (UNS-N08367), can it be used as a coil material inside a boiler(Complying with Sec I) ?
(OP)
Dear all,
I was asked the following question. Can anyone shade a light on it:
"AL-6XN (UNS-N08367), can this material be used as a coil material inside a boiler(Complying with Section I) ?
I was asked the following question. Can anyone shade a light on it:
"AL-6XN (UNS-N08367), can this material be used as a coil material inside a boiler(Complying with Section I) ?





RE: AL-6XN (UNS-N08367), can it be used as a coil material inside a boiler(Complying with Sec I) ?
RE: AL-6XN (UNS-N08367), can it be used as a coil material inside a boiler(Complying with Sec I) ?
RE: AL-6XN (UNS-N08367), can it be used as a coil material inside a boiler(Complying with Sec I) ?
= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
RE: AL-6XN (UNS-N08367), can it be used as a coil material inside a boiler(Complying with Sec I) ?
RE: AL-6XN (UNS-N08367), can it be used as a coil material inside a boiler(Complying with Sec I) ?
With long term exposure anything over 950F is dangerous.
= = = = = = = = = = = = = = = = = = = =
Plymouth Tube