INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Code & standard to repair damaged import center suction and Side entry mixer flanges

Code & standard to repair damaged import center suction and Side entry mixer flanges

Code & standard to repair damaged import center suction and Side entry mixer flanges

(OP)
Dear all,

Kindly help me to define which code and standard that require to be refer for the damaged flanges repair?

Thank
Marvin

RE: Code & standard to repair damaged import center suction and Side entry mixer flanges

I'm not aware of one but would like to know if one exists as well.

RE: Code & standard to repair damaged import center suction and Side entry mixer flanges

If 'plate flanges' [not forged, but cut from plate] fix to meet the requirements of API-650/653. If forged flanges ASME B16.5 allows some repairs; in general though, a damaged forging needs to be scrapped and replaced.

RE: Code & standard to repair damaged import center suction and Side entry mixer flanges

ASME PCC-1 or PCC-2 covers flange repair I thinks

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources