Hi gents,
I have PQR thickness 31.8mm, PWHT hoding time 3 Hour. Can I wirte WPS range hoding time 1 hour/1 inch
I have PQR thickness 31.8mm, PWHT hoding time 3 Hour. Can I wirte WPS range hoding time 1 hour/1 inch





RE: PWHT range time
Birken