Sbr-1500
Sbr-1500
(OP)
hey guys , I need your help please
I worked in a factory and we are using a copper greasing niplle and we want to replace it with a one made of Sbr-1500
the working conditions are
- NAOH 4% concentrating in water
- greasing with a lithium base
- Temperature up to 80 C
so could Sbr resist those condition
I worked in a factory and we are using a copper greasing niplle and we want to replace it with a one made of Sbr-1500
the working conditions are
- NAOH 4% concentrating in water
- greasing with a lithium base
- Temperature up to 80 C
so could Sbr resist those condition





RE: Sbr-1500
RE: Sbr-1500
but I think that NBR is much better, because the resistance to grease
here some useful link
http://www.jjshort.com/Rubber-Properties.php
RE: Sbr-1500
RE: Sbr-1500