INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Welder Qualification (Position) for Tank Shell Nozzles

Welder Qualification (Position) for Tank Shell Nozzles

Welder Qualification (Position) for Tank Shell Nozzles

(OP)

Good Day to all!,

I would like to request for clarification regarding the welder qualification (position) for API 650 Tank Nozzles

If a welder tested using a plate coupon in 2G & 3G position then he is qualified to weld both groove & fillet in F,H,V position as per QW-461.9. Can he weld shell nozzles with his current qualification?


Thanks

Kagemaru05

RE: Welder Qualification (Position) for Tank Shell Nozzles

How has the welder demonstrated their ability to place a weld in the overhead position? This would apply to the bottom of the nozzle neck to the shell. I would recommend qualifying the welder with an additional 4G or 5G position.

RE: Welder Qualification (Position) for Tank Shell Nozzles

Why not just qualify him on pipe in the 6G? This way he is completely covered for all diameters and positions for groove and fillets.

RE: Welder Qualification (Position) for Tank Shell Nozzles

(OP)
SectionIX and fegenbush

Thank you for your reply,our subcontractor wasn't able to qualify their welders for the overhead position so I have a doubt. Now I would recommend them for the 6G position.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources