INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

How can we inspect the equipment that protected with VCI(volatile corrosion inhibitor)?

How can we inspect the equipment that protected with VCI(volatile corrosion inhibitor)?

How can we inspect the equipment that protected with VCI(volatile corrosion inhibitor)?

(OP)
How can we inspect the equipment that protected with VCI(volatile corrosion inhibitor)?
for Periodic preventive maintenance of the equipments that store and protected with VCI internally, how should we do?
are there any standard or document about it?
thanks a lot.

RE: How can we inspect the equipment that protected with VCI(volatile corrosion inhibitor)?

Check the preservation procedure and review the inhibitor manufacturer's technical and safety data sheets regarding the necessary activities for unsealing and resealing the equipment.

Steve Jones
Corrosion Management Consultant

http://www.linkedin.com/pub/8/83b/b04

All answers are personal opinions only and are in no way connected with any employer.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources