(OP)
Hey guys I'm new to the rubber business I have some extrusion that just rips apart just be pulling it at it...
Inital investigation makes me think it is overcured but are there any other causes I need to investigate?
Inital investigation makes me think it is overcured but are there any other causes I need to investigate?





RE: extruded sponge EPDM tears easy...
RE: extruded sponge EPDM tears easy...