INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Where can I purchase/Order GLARE samples

Where can I purchase/Order GLARE samples

Where can I purchase/Order GLARE samples

(OP)
Does anyone know where I can get/buy some GLARE material samples for my tests ?

RE: Where can I purchase/Order GLARE samples

http://en.wikipedia.org/wiki/GLARE

Regards, Wil Taylor

Trust - But Verify!

We believe to be true what we prefer to be true.

For those who believe, no proof is required; for those who cannot believe, no proof is possible.

RE: Where can I purchase/Order GLARE samples

(OP)
Thanks wktaylor , but the wikipeida company name mentioned Cytec does not produce GLARE itself but rather provide the epoxy and resin that is used to produce GLARE smile

Cheers

RE: Where can I purchase/Order GLARE samples

GLARE is currently produced by Cytec Engineered Materials in Wrexham, UK who supplies it to the Airbus A380 component manufacturing facilities at Stork Fokker in the Netherlands as well as at Airbus in Nordenham, Germany. Stork Fokker has opened a brand new facility next to its existing facilities in Papendrecht, the Netherlands. There Stork Fokker is able to produce Glare sheets of 4.5 x 11.5 m including the milling of doors windows etc. on a state-of-the-art 5-axis milling machine with a movable bed. See attached TDS.

GLARE Configurations
Designation Aluminum Fiber Orientation
GLARE-I 7075-T6 Unidirectional*
GLARE-2 2024-T3 Unidirectional*
GIARE-3 2024-T3 50/50 % Crossply
GLARE-4 2024--T3 70/30 % Crossply

These are places to start "calling".
---------------------------------------------------------
Some interesting tech reports on GLARE ...

OPEN HOLE MULTILAYER FATIGUE CRACK GROWTH IN GLARE UNDER COMBINED TENSION BENDING
http://www.dtic.mil/dtic/tr/fulltext/u2/a433899.pd...

WL-TR-94-3134 DAMAGE TOLERANT REPAIR TECHNIQUES FOR PRESSURIZED AIRCRAFT FUSELAGES
http://www.dtic.mil/dtic/tr/fulltext/u2/a286298.pd...

AFIT/DS/ENY/97-4 Thickness Effects on a Cracked Aluminum Plate with Composite Patch Repair
http://www.dtic.mil/dtic/tr/fulltext/u2/a327983.pd...

AFIT Thesis MECHANICAL PROPERTIES CHARACTERIZATION AND BUSINESS CASE ANALYSIS OF THE FIBER METAL LAMINATE GLARE-3 FOR USE AS A SECONDARY AIRCRAFT STRUCTURE
http://www.dtic.mil/dtic/tr/fulltext/u2/a521800.pd...


Regards, Wil Taylor

Trust - But Verify!

We believe to be true what we prefer to be true.

For those who believe, no proof is required; for those who cannot believe, no proof is possible.

RE: Where can I purchase/Order GLARE samples

(OP)
Thanks a lot Wil Taylor smile, I have already emailed them and I am waiting for their reply to confirm about whether they could provide me with GLARE

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources