INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

API 5L material X46
3

API 5L material X46

API 5L material X46

(OP)
Dear all,

I am looking for material for flange which suitable for API 5L X46 pipe class.
My customer ask casted material and they sent me this:

ASTM A494 F46

I have not found any F46 in this material spec.

Can you recomended something?

Thank you

RE: API 5L material X46

2
I think this is a typo. Try A 694.

My motto: Learn something new every day

Also: There's usually a good reason why everyone does it that way

RE: API 5L material X46

(OP)
Thank you very much.
I spent hours on it.

Regrads

elmio

RE: API 5L material X46

Hi.

The material must be A694 F46.

greetings to all.

RE: API 5L material X46

(OP)
Thank you hfpolo!

It was a typing error by customer. Our sales team did enough mistake that case I did not want ask back to the customer.

Regards

Elmio

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources