Crevice Factor
Crevice Factor
(OP)
Our customer wants duplex castings with PREn >=40 and "Crevice Factor" >35. We regularly produce alloy CE8MN with PREn >=40, but I have not heard of or used a "Crevice Factor". Can anyone point me to information on how to calculate or test for this property?
Thanks
CE8MN
Thanks
CE8MN





RE: Crevice Factor
Crevice factor on eng-tips.com
RE: Crevice Factor
http://tools.outokumpu.com/spt/pub/upload/pubs_122...
Steve Jones
Corrosion Management Consultant
http://www.linkedin.com/pub/8/83b/b04
All answers are personal opinions only and are in no way connected with any employer.
RE: Crevice Factor
Steve Jones
Corrosion Management Consultant
http://www.linkedin.com/pub/8/83b/b04
All answers are personal opinions only and are in no way connected with any employer.