INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

The difference on FTPR and Viton + valve question

The difference on FTPR and Viton + valve question

The difference on FTPR and Viton + valve question

(OP)
I have some valves that will be placed in pipes with following service:
Lemon acid, base (type caustic soda) and biocide.

1.
In the valve data cheet, they say that PTFE shall be used as sealing material in the valve. The supplier offers VITON.
2.
It also says that the stuffing box shall consist of expanded graphite not less than 98 % purity.
The supplier offers: TFE + 25% C. Graphite

Is there anyone that knows if I can accept this or do I have to correct the valves?

Is there someone who know what the difference is between FTPR and VITON?

RE: The difference on FTPR and Viton + valve question

Viton is a tradename for a variety of fluoropolymers manufactured by DuPont Dow Elastomers.  You can obtain more information about the various grades at the following website:

http://www.dupont-dow.com/Products/Viton/viton.asp


PTFE is an acronym for Polytetrafluoroethylene.
TFE is just PTFE without the P at the beginning.
I do not know what FTPR is.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources