% of Al in 6061
% of Al in 6061
(OP)
Does anyone have a nominal figure for how much Al is in the composition of 6061 alloy?
I worked out 95.5% from my datasheets but would like a second opinion.
Thanks
I worked out 95.5% from my datasheets but would like a second opinion.
Thanks





RE: % of Al in 6061
Remainder Aluminium (95.85%–98.56%)
rp