INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

ASME B31.3

ASME B31.3

ASME B31.3

(OP)
I need some help determining the acceptable limits of porosity in B31.3 normal fluid service.

Criterion Value Notes for Table 341.3.2

D Size and distribution of internal porosity See BPV Code, Section VIII, Division 1, Appendix 4
E Size and distribution of internal porosity
For T w ≤ 6 mm (1⁄4 in.), limit is same as D
For T w > 6 mm (1⁄4 in.), limit is 1.5  D

Im having trouble interpting what this means and the code it need to reference to.


Thanks,
Tommy

RE: ASME B31.3

The code this refers to is ASME B&PV Code Section VIII, Div 1, Appendix 4. Appendix 4 is titled

MANDATORY APPENDIX 4
ROUNDED INDICATIONS CHARTS
ACCEPTANCE STANDARD FOR
RADIOGRAPHICALLY DETERMINED
ROUNDED INDICATIONS IN WELDS

If you don't have Appendix 4 of the code you have a problem.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources