I'm looking for plastics that can transmit UV-C Hopefully down to about 150nm. Thanks for any suggestions,
Don
Don
When was the last time you drove down the highway without seeing a commercial truck hauling goods?
Download nowINTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
Plastics That Can Transmit UV-C
|
RE: Plastics That Can Transmit UV-C
http://www.lrsm.upenn.edu/~frenchrh/download/0807J...
Note most people think Teflon (TM) is the same as PTFE. In fact DuPont use the Teflon brand name for several fluoropolymers.
Dr. Chris DeArmitt - FRSC
www.linkedin.com/in/chrisdearmitt/
RE: Plastics That Can Transmit UV-C