INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

QW-103.1: Manufacturer

QW-103.1: Manufacturer

QW-103.1: Manufacturer

(OP)
Are procedure qualififications restricted to a particular site of a qualified manufacturer or can they be given back and forth between manufacturers of the same company?

RE: QW-103.1: Manufacturer

What does your QA/QC manual state? Are sites controlled by a single location (Corp) or do sites control their own welding procedures?

RE: QW-103.1: Manufacturer


The Code recognizes a manufacturer or contractor as
the organization which has responsible operational control
of the production of the weldments to be made in accordance
with this Code. If in an organization effective operational
control of welding procedure qualification for two
or more companies of different names exists, the companies
involved shall describe in their Quality Control
system/Quality Assurance Program, the operational control
of procedure qualifications. In this case separate welding
procedure qualifications are not required, provided all other
requirements of Section IX are met.

Nasir
Welding Engineer
DESCON ENGINEERING LIMITED
PAKISTAN

RE: QW-103.1: Manufacturer

(OP)
Metengr
Our site controls our own procedures, so it seems that each site has to weld a procedure qual. Is this correct?

RE: QW-103.1: Manufacturer

Yes each site has to qualify his own procedures because operational control is not centralized and no so stated in quality control system.

Nasir
Welding Engineer
DESCON ENGINEERING LIMITED
PAKISTAN

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources