INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

RMS 042 Type 2 Grade B film adhesive

RMS 042 Type 2 Grade B film adhesive

RMS 042 Type 2 Grade B film adhesive

(OP)
I am trying to find what adhesives fall under the RMS 042 spec for Type 2 Grade B .005" adhesives. Any help would be appreciated as I have not been able to find RMS specs anywhere.

HibbyJ

RE: RMS 042 Type 2 Grade B film adhesive

ROHR: RMS 042, Type 2, Grade B (as of 2003)

3M: AF-15, .015 - .019PSF unsupported Film Adhesive. (0.003" =/- 0.001")
Per 3M Tech Support, use AF-31 Tech Data Sheet.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources