Material Stress Values for SA201-A at 100F and 825 F and SA201-B at 100F and 500F?
Material Stress Values for SA201-A at 100F and 825 F and SA201-B at 100F and 500F?
(OP)
Hello
I need to work on some old vessels and require the allowable stresses of SA201-A at 100F and 825F and SA201-B at 100F and 500F, Can anyone help?
Thanks in advance
Tomtation
I need to work on some old vessels and require the allowable stresses of SA201-A at 100F and 825F and SA201-B at 100F and 500F, Can anyone help?
Thanks in advance
Tomtation





RE: Material Stress Values for SA201-A at 100F and 825 F and SA201-B at 100F and 500F?
100 deg F 13,750 psi
800 deg F 10,200 psi
100 deg F 15,000 psi
500 deg F 15,000 psi
RE: Material Stress Values for SA201-A at 100F and 825 F and SA201-B at 100F and 500F?
RE: Material Stress Values for SA201-A at 100F and 825 F and SA201-B at 100F and 500F?