INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

HDPE Pipe Coils

HDPE Pipe Coils

HDPE Pipe Coils

(OP)
As a part of designing a water distribution system in Uganda, my university's chapter of Engineers Without Borders requires to analyze the safety concerns regarding the pipe coils and related handling. The data I got off the internet was too generic, and if the group community can be specific, it would be greatly appreciated.
The question is about uncoiling the HDPE pipes (length 100 m, outer diameters variable ranging from 25 mm to 90 mm, PE-100 raw material and pressure rating of PN-16). Do industry wound pipe coils pose a threat to the person trying to uncoil it by exerting large forces? If yes, is manual uncoiling possible at all? Also, if not, does HDPE resist uncoiling, in which case force would be required to uncoil it? Because of the financial constraints, most of the labor work would be manual with minimal tools. Any other suggestions regarding the same would be valuable also.
Thank you!

RE: HDPE Pipe Coils

I would consider redflagging this post, and re-posting it in the "Mechanical Engineering>Pipelines, Piping and Fluid Mechanics Engr." forum. There are people there with a lot of experience in laying large-diameter HDPE pipelines. FWIW, I have laid 1" poly pipe, but the bigger stuff makes me nervous.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.