INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

BS 3146 Part1 CLA 11

BS 3146 Part1 CLA 11

BS 3146 Part1 CLA 11

(OP)
Any recommended cast materials (Ni or Co base) to use for the oilfield drilling (turbodrilling motors) with similar properties to BS3146 Part 1 CLA 11 (nitriding steel)?

RE: BS 3146 Part1 CLA 11

Unfortunately, I do not have a copy of this BS specification.  Can you please provide the chemical composition, as well as the strength/hardness requirements?  My first impression is that you do want to change to a Ni or Co-based alloy because the wear resistance will be greatly inferior to that of a nitrided steel alloy.  Can you provide some additional details, such as your reasoning for changing to Ni or Co-based alloys?  Expected operating environment, etc.?

RE: BS 3146 Part1 CLA 11

(OP)
BS 3146 Part 1 CLA 11 covers castings with 3% Cr-Mo nitriding steel (alloy similar BS 970 - 722M24.)
Analysis
C 0.20/0.30
Si 0.3/0.8
Mn 0.3/0.6
S & P 0.035 max
Cr 2.9/3.5
Mo 0.4/0.7
Ni 0.4 max
Cu .3 max
V  .02 max
Sn .03 max
Mech prop (min)
TEN. STRENGTH 924 N/MM2
YIELD STRESS  780 N/MM2
ELONG 17.1%
BHN  269

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources