Can anyone provide information regarding the applicability and certification of bronze valves to NACE 0175?
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
|
RE: NACE 0175 - bronze
For certification: thread338-264003: valves who meet NACE MR 0175
Steve Jones
Materials & Corrosion Engineer
http://www.linkedin.com/pub/8/83b/b04
All answers are personal opinions only and are in no way connected with any employer.