INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Solid Tungsten Carbide Stem Tip for Choke Valve (Well Head area)

Solid Tungsten Carbide Stem Tip for Choke Valve (Well Head area)

Solid Tungsten Carbide Stem Tip for Choke Valve (Well Head area)

(OP)
ISO 15156-3 does not list Tungsten Carbide as one of the qualified material, but it is observed most of the Choke Valve suppliers offer Tungsten carbide Stem Tip (Needle tip) as Solid Tungsten Carbide. It is alomost an industry practice.

Also it is understood this Solid Tungsten Carbide is HIP product form using Cobalt as binder.

My questions are

1) Does NACE MR 0175/ISO 15156 permit the use of Solid Tungsten Carbide Stem tip/ Cage without SSCC qualification testing?

2) Are there restrictions in Hardness and Chemistry for Solid Tungsten Carbide

3) API 6A does not specify any NDE (In fact there is an indicator of exclusion) or QC test for the stem tip solid tungsten Carbide, is there any ISO or ASTM standard or any world standard/code that gives recommendations (Client specific wish list not required) for HIP product forms?


Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources