7075 T73 9" OD extruded forged
7075 T73 9" OD extruded forged
(OP)
I need to procure 7075 T73 9" OD. I have noticed some extrusion specs like ASTM B221 don't specify mech props beyond 4.5". Should I specify open die forging instead of extrusion to get the size I need with consistent properties?