Can extrusion be good on one end and pitted in the middle section?
Can extrusion be good on one end and pitted in the middle section?
(OP)
Have here Aluminum extrused parts that are pitted.
Seems like material problem, but the same lot of material ran fine a month ago.
Seems like material problem, but the same lot of material ran fine a month ago.





RE: Can extrusion be good on one end and pitted in the middle section?
RE: Can extrusion be good on one end and pitted in the middle section?
RE: Can extrusion be good on one end and pitted in the middle section?
More info needed.