What is the English Equivalent to S
What is the English Equivalent to S
(OP)
What is the English Equivalent to SS 2172-03 & SS 2134-04
Discover the role technology plays in supporting transformation and the importance of Engineering and Manufacturing collaboration
Download NowINTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
What is the English Equivalent to S
|
RE: What is the English Equivalent to S
SS 2134-04 --> S355NH according to BS EN 10210-1