subsea temp sensor
subsea temp sensor
(OP)
Hi friend
I have subsea temp sensor type TX486-0130 RANGE 0 ~ 100C use in conjunction with separate 300 mm .long nosed API.6A flanged thermo well type 4FLG-014X
MADE BY LUCAS VARITY no more exist, aquired by rtw company, and the product no more produced
Anyone can suggest for me the replacement
I have subsea temp sensor type TX486-0130 RANGE 0 ~ 100C use in conjunction with separate 300 mm .long nosed API.6A flanged thermo well type 4FLG-014X
MADE BY LUCAS VARITY no more exist, aquired by rtw company, and the product no more produced
Anyone can suggest for me the replacement
If you can dream it you can do it





RE: subsea temp sensor
If you need high accuracy specify a 4 wire sensor.
I think Monel is a suitable material for the well in seawater.
Roy
RE: subsea temp sensor