INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

ASME design issue

ASME design issue

ASME design issue

(OP)
Hellow,
Our company builds piping enclosures for industrial plants. We designg these to asme section VIII and b31.3. Can anyone explain more in dept between the joint efficiency factor and the design efficiency per asme code. Im trying to desing the proper weld pentration per ASME code which our calcs require 70%

Thanks,
Tommy

RE: ASME design issue

If you have a copy of ASME Section VIII, Div 1 please review UW-12 and Table UW-12. It really is self explanatory. For B31.3 review paragraph 302.3.4 and associated Table 302.3.4.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources