INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Steel S275 Plastic Properties

Steel S275 Plastic Properties

Steel S275 Plastic Properties

(OP)
Hi all,

I need to implement the plastic properties of the Steel S275 for a non-linear simulation and I just found properties for a random steel that are:
Yield Stress Plastic Strain
200 0
246 0.0235
294 0.0474
374 0.0935
437 0.1377
480 0.18

Do anyone know the properties for S275 or if the results with that one will differ too much?

Thanks

RE: Steel S275 Plastic Properties

You can input TRUE stress-strain S275 data according to Eurocode 3.
If you need real relationship beetwen stress and strain for S275 steel I recommend You to search a tensile test and results on the internet.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources