material for support stand for caustic tote bins
material for support stand for caustic tote bins
(OP)
Good day folks,
We are looking to fabricate a support stand for a tote bin containing caustic material.
I'm looking into the use of Alloy 20 for the support stand but of course the cost might be of the charts.
Can anyone provide some suggestions on materials which we can use to bear the sulfuric acid?
Any information provided will be greatly appreciated.
Thanks.
We are looking to fabricate a support stand for a tote bin containing caustic material.
I'm looking into the use of Alloy 20 for the support stand but of course the cost might be of the charts.
Can anyone provide some suggestions on materials which we can use to bear the sulfuric acid?
Any information provided will be greatly appreciated.
Thanks.






RE: material for support stand for caustic tote bins
Mike McCann
MMC Engineering
http://mmcengineering.tripod.com
RE: material for support stand for caustic tote bins
Check into fiberglass, maybe?