INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

can you solution treat ASTM A193 B8m class 2 solution treated and strain hardened to B8MA class 1

can you solution treat ASTM A193 B8m class 2 solution treated and strain hardened to B8MA class 1

can you solution treat ASTM A193 B8m class 2 solution treated and strain hardened to B8MA class 1

(OP)
Just wondered if you have some B8m class 2 material would you be able to solution treat it so to conforms to B8MA

RE: can you solution treat ASTM A193 B8m class 2 solution treated and strain hardened to B8MA class 1

I don't see anything in ASTM A193 that prohibits this. Distortion of the shank/thread may be an issue.

RE: can you solution treat ASTM A193 B8m class 2 solution treated and strain hardened to B8MA class 1

I would agree with TVP, and have the same reservations about distortion.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources