Sulphuric Acid Specifications
Sulphuric Acid Specifications
(OP)
Dear All,
Anyone of you have came across with the following sulphuric acid specifications in the market:
H2SO4 = 98 wt%
Chlorides as Cl = <40 mg/kg
Fe = <50 mg/kg
NO2 = <50 mg/kg
SO2 = <15 mg/kg
As = <0.1 mg/kg
Hg = <0.1 mg/kg
Urgent reply is highly appreciated. Thanks!
Anyone of you have came across with the following sulphuric acid specifications in the market:
H2SO4 = 98 wt%
Chlorides as Cl = <40 mg/kg
Fe = <50 mg/kg
NO2 = <50 mg/kg
SO2 = <15 mg/kg
As = <0.1 mg/kg
Hg = <0.1 mg/kg
Urgent reply is highly appreciated. Thanks!





RE: Sulphuric Acid Specifications
These are pretty typical specifications for 98 wt% sulfuric acid.
Some of the "trace" components may not be specified in the standard specifications of the usual suppliers, but I am sure they could be provided if that is what you are after.