API 5L grade B PSL2 in US?
API 5L grade B PSL2 in US?
(OP)
Hello I am trying to order replacement pipe with flanges to match current pipe system. The diameter is 28" and i am having diffulcutly in flange specification. Also I require PSL2 and am having a problem locating a vendor in the US. Can I use a PSL1 or other suggestions or purchase from outside US?
Use pipe spec - API 5L Gr. B. PSL-2, DSAW Flange spec - ASTM A105N, Class
150 RF. WN B16.47-A (Bore to match pipe)
Use pipe spec - API 5L Gr. B. PSL-2, DSAW Flange spec - ASTM A105N, Class
150 RF. WN B16.47-A (Bore to match pipe)





RE: API 5L grade B PSL2 in US?
Flange spec - ASTM A105N Class 150 RF. WN B16.47-A (Bore to match pipe)