Round Bar to Pipe WPS
Round Bar to Pipe WPS
(OP)
Hello All,
So sort of new to WPS and prequalification of procedures, however I am required to have one for welding round bar to piles. This is something that we have done for years but have never been required to have a procedure for... well at least not to my knowledge.
Here is the detail of the joint: SMAW procedure welding 1" Diam Round Bar Double Flare-Bevel-Groove Weld to a 14" Diam x 0.375" Wall Pipe Pile.
From what I have read in D1.1 in Clause 3 there is no Prequalified WPS for this certain situation (unless I am missing something. I studied joint designation BTC-P10 Page 84 of the 2010 D1.1 book, but that is the closes I could find to the joint but it wont work.
Any suggestion of where to go from here?
Thanks in advance!
So sort of new to WPS and prequalification of procedures, however I am required to have one for welding round bar to piles. This is something that we have done for years but have never been required to have a procedure for... well at least not to my knowledge.
Here is the detail of the joint: SMAW procedure welding 1" Diam Round Bar Double Flare-Bevel-Groove Weld to a 14" Diam x 0.375" Wall Pipe Pile.
From what I have read in D1.1 in Clause 3 there is no Prequalified WPS for this certain situation (unless I am missing something. I studied joint designation BTC-P10 Page 84 of the 2010 D1.1 book, but that is the closes I could find to the joint but it wont work.
Any suggestion of where to go from here?
Thanks in advance!





RE: Round Bar to Pipe WPS
The size of the weld, thus the load it can transfer is limited by Table 2.1.
Best regards - Al