Sulfur content
Sulfur content
(OP)
Gents,
We have carried out lab test for API 5CT L-80 (13%) material and found that sulfur content is 0.012% wheras API 5CT restricts it to 0.010%. Can we accept this? Also, I would like to know the difference between ppm and % mass fraction in pertaining to chemical composition.
Regards
We have carried out lab test for API 5CT L-80 (13%) material and found that sulfur content is 0.012% wheras API 5CT restricts it to 0.010%. Can we accept this? Also, I would like to know the difference between ppm and % mass fraction in pertaining to chemical composition.
Regards





RE: Sulfur content
RE: Sulfur content
Regards
RE: Sulfur content
What was the method for chemical analysis? I am referring to either an ASTM Standard or other international standard. There are product analysis methods and reporting accuracy. Please obtain a copy and READ ASTM A 751. Keep in mind there is a line to be drawn when evaluating materials for conformance or nonconformance and if your product ends up on the other side of the line, so be it.
RE: Sulfur content
Look it up.
= = = = = = = = = = = = = = = = = = = =
Plymouth Tube