AWS D1.1 Table 4.5 # 34-Essential Variable Clarification
AWS D1.1 Table 4.5 # 34-Essential Variable Clarification
(OP)
hello people
so referring back to this thread - http://www.eng-tips.com/viewthread.cfm?qid=315118 - if i have a pqr that qualifies a double sided cjp with backgouging and the wps refers to a single sided cjp with backing strip without backgouging is the wps applicable and does this comply under the code?
thanks





RE: AWS D1.1 Table 4.5 # 34-Essential Variable Clarification
Best regards - Al
RE: AWS D1.1 Table 4.5 # 34-Essential Variable Clarification
RE: AWS D1.1 Table 4.5 # 34-Essential Variable Clarification
Regarding backing and back gouging: can they be used interchangeably ? In other word : can we use PQR with backing to weld with back gouging or vice versa ?
RE: AWS D1.1 Table 4.5 # 34-Essential Variable Clarification
RE: AWS D1.1 Table 4.5 # 34-Essential Variable Clarification
Best regards - Al