ISO 15164 table 5 note a
ISO 15164 table 5 note a
(OP)
I have a question on how to understanding ISO 15164 table 5 note a: when impact requirements are specified the upper limit of qualification is 12mm unless impact testing has been performed.
All of our products needs to pass the impact test. Structure steel involved here.
if a test pieces is 10mm thick on the WPQR, it will qualify the WPS with thickness of 3-12mm.
If I need to qualify a WPS with the range of 3-20mm, I have to do a impact testing on the testing sample of 20mm.
is this the correct understanding?
Or, another understanding can be to do a test on the 10mm plate. but if so, the "note a" is unnecessary.
how shall i understand it? Someone help me please!
All of our products needs to pass the impact test. Structure steel involved here.
if a test pieces is 10mm thick on the WPQR, it will qualify the WPS with thickness of 3-12mm.
If I need to qualify a WPS with the range of 3-20mm, I have to do a impact testing on the testing sample of 20mm.
is this the correct understanding?
Or, another understanding can be to do a test on the 10mm plate. but if so, the "note a" is unnecessary.
how shall i understand it? Someone help me please!





RE: ISO 15164 table 5 note a
RE: ISO 15164 table 5 note a
Steve Jones
Materials & Corrosion Engineer
http://www.linkedin.com/pub/8/83b/b04
RE: ISO 15164 table 5 note a