INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Norsok - filling in the I-datasheet L05 - what is required under 1.08 Sour service specification?

Norsok - filling in the I-datasheet L05 - what is required under 1.08 Sour service specification?

Norsok - filling in the I-datasheet L05 - what is required under 1.08 Sour service specification?

(OP)
Hello,
I have just joined. Have found this forum helpful many times :)

I work more and more with documentation, and are learning by doing.
Now I am working my way through a Norsok datasheet L05 for a gauge.
1.08 sour service specificitaion - What type of information is expected here?

I have googled but have not found any clear answer....

Hoping some of you know :)

Regards
Irene

RE: Norsok - filling in the I-datasheet L05 - what is required under 1.08 Sour service specification?

Try researching ISO 15156 or NACE MR0175. It may also help to indicate which NORSOK standard L05 belongs to. At the moment, we will assume I-001.

Steve Jones
Materials & Corrosion Engineer

http://www.linkedin.com/pub/8/83b/b04

RE: Norsok - filling in the I-datasheet L05 - what is required under 1.08 Sour service specification?

(OP)
Thank you.
Yes that is correct: It belongs to I-001 :)

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources