Safe temperature for carbon steel
Safe temperature for carbon steel
(OP)
What temperature will be considered to be safe for carbon steel for continuous heating application ? If it is heated continuously/intermittently to 300 degrees centigrade, is there any metallurgical deterioration ?





RE: Safe temperature for carbon steel
RE: Safe temperature for carbon steel
RE: Safe temperature for carbon steel
No. Carbon steel at 500 deg C will exhibit creep deformation under load and will oxidize in air.