INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

AWS D1.1 Diffusible Hydrogen H values

AWS D1.1 Diffusible Hydrogen H values

AWS D1.1 Diffusible Hydrogen H values

(OP)
Exactly where are the H values (for hydrogen) shown in AWS D1.1 for various steels and electrodes I am looking at all the tables, and not seeing this. I am preparing for the ICC Welding exam (S2), and a sample test question asks, using ASTM A913
steel > 1.50 inches, no preheat, what is the max diffusible hydrogen H value to be used

RE: AWS D1.1 Diffusible Hydrogen H values

It isn't in the body, i.e.lauses 1 through 8, of D1.1

Al

Best regards - Al

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources