EN8D axle shafts temper time
EN8D axle shafts temper time
(OP)
We do induction heat treatment of axle shafts made of EN8D and then furnace temper it.Axle shafts are 58-62 HRC as quenched.for how much time and at what temperature we temper them to get 55-56HRC on surface?





RE: EN8D axle shafts temper time
RE: EN8D axle shafts temper time
RE: EN8D axle shafts temper time
_____________________________________
"It's better to die standing than live your whole life on the knees" by Peter Mayle in his book A Good Year