INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Expansion Joints in Mat Foundations?

Expansion Joints in Mat Foundations?

Expansion Joints in Mat Foundations?

(OP)
Do large Mat foundations require expansion joints?

RE: Expansion Joints in Mat Foundations?

Good afternoon gramy13,

Not normally (contraction/shrinkage is more the issue). They will have construction joints if necessary but are often placed continuously. Making provisions for heat of hydration need to be considered and can involve slowing hydration with special mixes using slag cement and/or fly ash. Cooling tubes are sometimes used although not as often as they were at one time.

regards,
Michel

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources